What this guide covers

Everything we get asked about timber coatings, in one place: what the different coating families actually are, how curing works and why it decides your programme, how to work out what a job needs, and how to apply it. Each section links to the guide that goes deeper on it, and to the projects where the system has been used.

Most coating decisions get made on price per litre and a photograph of a finished floor. Neither tells you much. What actually determines whether a job runs well is how the finish cures, what it puts into the air while it does, and how far it goes.

The coating families

Most timber finishes fall into two camps. Film finishes, meaning lacquers and varnishes, sit on top of the timber as a layer. Penetrating finishes, meaning oils and hardwax oils, soak into the timber and leave a thin protective layer rather than a skin.

The practical difference shows up when something gets damaged. A film finish breaks, and the break has edges, so repairs usually mean taking the whole area back. A penetrating finish wears thin rather than breaking, which is why an oiled floor can be cleaned, re-oiled and blended without stripping it.

Then there are the terms that describe where and how a finish was cured rather than what it is made of, which is where most of the confusion lives. UV oiled means a hardwax oil cured under lamps in a factory before the boards were delivered. LED cured means a coating that hardens under light on site, as it is applied.

Read: what is the difference between UV and LED curing?

How curing works, and why it sets your programme

A conventional oil hardens by reacting with oxygen in the air. That takes hours to become touch dry and days to harden properly, and it slows down further when it is cold or humid. A conventional lacquer hardens as its solvent evaporates, which has the same consequence: time.

Energy curing works differently. A specific wavelength of light, 395nm in our case, triggers the coating to cross-link on contact. The film is fully hard as the lamp passes over it, not touch dry. Nothing has to evaporate and nothing has to react with the air.

That one difference removes the waiting, and the waiting is where most of the real cost sits: racks occupied, floor space tied up, a room that cannot be used, a handover date that slips because the finish was not ready rather than because the work was not done.

Read: the real cost of slow drying coatings

What a coating puts into the air

A solvent based finish dries by evaporation, and what evaporates is the solvent. Those compounds are volatile organic compounds, and they keep leaving the film for days after the surface feels dry to touch. In an enclosed workshop the concentration builds up quickly and stays up.

A coating that cures under light has nothing to evaporate, because nothing has to leave the film for it to harden. That is the difference between a finish you can only use in an empty, well ventilated space and one you can use in a school, a clinic, an office or a home that people are still living in.

Read: clearing the air on VOCs

Working out what a job needs

Hardwax oil is sold by the litre and used by the square metre, which is why the price on the tin tells you very little on its own. A tin at half the price with half the coverage costs you the same, and a tin at half the price with a third of the coverage costs you more.

Most hardwax oils cover 20 to 30 square metres per litre, and most data sheets quote that figure per coat while specifying two coats. Oslek LED Hardwax Oil covers 40 to 50 square metres per litre by hand, or 70 to 80 by machine. Multiply it out before comparing anything.

Step What to do
1 Measure the area in square metres
2 Divide by the coverage per litre from the data sheet
3 Multiply by the number of coats
4 Add about 10 per cent for waste and edges

Read: how much hardwax oil do you actually need?

Applying it

The method differs between a floor and a workbench, mostly in the equipment and in how the oil is worked into the surface. Both follow the same principle: prepare evenly, apply sparingly, work it in, take the excess off, then cure.

Over-application causes more finish failures than everything else combined. Hardwax oil is meant to penetrate, and anything the timber cannot absorb sits on the surface with nothing to react with.

Made here

We are a family business with more than fifteen years in the timber industry. What began as a flooring company became a coatings manufacturer, and we make the product ourselves in Melbourne. Everything from research and pigment mixing through to full scale production happens in house.

Vertical integration is not easy, but it means tighter quality control, consistent performance batch to batch, and a product we stand behind from start to finish. It also means that when a specifier rings with a colour match or a difficult substrate, the people who made the coating are the people answering.

Seeing it in use

Retail, hospitality and residential projects finished with Oslek LED Hardwax Oil, including European oak herringbone, custom colour matched floors, cork panelling and furniture.

  • Camilla and Marc, ArmadaleEuropean oak herringbone in a heritage terrace boutique, finished in a custom grey oil. Winner of an Australian Interior Design Award.
  • Camilla and Marc, BondiCustom stained oak herringbone running alongside terrazzo tiling in a flagship store.
  • The Panel HouseEuropean oak flooring in a 950 square metre certified Passivhaus Premium home, chosen for indoor air quality.
  • Aesop, DoncasterCork wall panels finished in LED Hardwax Oil Clear and cured in place on site.
  • Rifle RangeTimber wall panelling and ceiling features in a passive house retrofit.
  • NewNewA modular pavilion built on circular design principles, finished so the timber can be refinished and reused.
  • Stay StoolA reissued Tom Skeehan design, finished for everyday use on a timber and steel frame.

Browse the project case studies

Common questions

What is the difference between hardwax oil and lacquer?

A lacquer forms a film on top of the timber. A hardwax oil penetrates it and leaves a thin protective layer. The practical consequence is repairability: a lacquer breaks and usually needs taking back, while an oiled surface wears thin and can be cleaned, re-oiled and blended.

How long before a newly finished floor can be used?

It depends entirely on the coating. A conventional hardwax oil is typically touch dry in hours and fully cured in days. An LED cured coating is walkable as soon as the lamp has passed over it.

Can timber be refinished in an occupied building?

Yes, with the right finish and sensible phasing. The limiting factors are odour and drying time rather than the sanding itself. A solvent free finish that cures on contact can be handed back the same day.

Does a more expensive coating cost more per square metre?

Not necessarily, and often the opposite. Price per litre only means something once you divide it by coverage and multiply by the number of coats the data sheet specifies.

How much does LED Hardwax Oil cover?

40 to 50 square metres per litre applied by hand, or 70 to 80 by machine. That is roughly double to triple a typical hardwax oil, which is why comparing per litre prices is misleading.

Try it before you commit

Most people start with a sample. Coat a piece of timber, cure it under the lamp, and see in seconds what the rest of this guide describes. Then order the full size when you are ready.